Communicate with Supplier? Supplier
Allen Zhu Mr. Allen Zhu
What can I do for you?
Contact Supplier

Seonjip

HomeProductsDeforming SuperalloyNimonic alloy 80A round bar rod

Nimonic alloy 80A round bar rod

  • $20
    ≥100
    Kilogram
Payment Type:
L/C,T/T,D/P,D/A,Paypal,Money Gram,Western Union
Incoterm:
FOB,CFR,CIF,EXW
Min. Order:
100 Kilogram
Transportation:
Ocean,Land,Air,Express
Port:
any port in China
Share:
  • Product Description
Overview
Product Attributes

Model No.Nickel Bar

place of originChina

Powder Or NotNot Powder

ApplicationIndustry, Construction,Boiler Pipe

GradeNickle Alloy

Ni (Min)Stable

Resistance (μΩ.m)Stable

Supply Ability & Additional Informations

PackagingProducts are well packed and clear labeled according to the regulations and customer's requests

TransportationOcean,Land,Air,Express

Supply Ability3000 Ton/Tons per Month

Portany port in China

Payment TypeL/C,T/T,D/P,D/A,Paypal,Money Gram,Western Union

IncotermFOB,CFR,CIF,EXW

Packaging & Delivery
Selling Units:
Kilogram
Package Type:
Products are well packed and clear labeled according to the regulations and customer's requests
Picture Example:

High temperature alloy has the high temperature hot corrosion and high temperature abrasion resistance,the metal material can work long-term which above 600 ℃ with under certain stress conditions.

Product Name Nimonic Alloy 80A round bar rod

Material Monel/Inconel/Hastelloy/Duplex Steel/PH Steel/Nickel Alloy

Shape Round,Forging,Ring,Coil,Flange,Disc,Foil,Spherical,Ribbon,Square,Bar,Pipe,Sheet

Grade Duplex: 2205(UNS S31803/S32205),2507(UNS S32750),UNS S32760(Zeron 100),2304,904L

Others: 253Ma,254SMo,654SMo,F50(UNS S32100)F60,F61,F65,1J22,N4,N6 etc

Alloy : Alloy 20/28/31;

Hastelloy: Hastelloy B/ -2/B-3/C22/C-4/S/ C276/C-2000/G-35/G-30/X/N/g;

Hastelloy B / UNS N10001,Hastelloy B-2 / UNS N10665 / DIN W. Nr. 2.4617,Hastelloy C,Hastelloy C-4 /

UNS N06455 / DIN W. Nr. 2.4610,Hastelloy C-22 / UNS N06022 / DIN W. Nr. 2.4602,Hastelloy C-276 / UNS N10276 / DIN W. Nr. 2.4819,Hastelloy X / UNS N06002 / DIN W. Nr. 2.4665

Haynes: Haynes 230/556/188;

Inconel Series:

Inconel 600/601/602CA/617/625/713/718/738/X-750,Carpenter 20;

Inconel 718 / UNS N07718 / DIN W. Nr. 2.4668,Inconel 601 / UNS N06601 / DIN W. Nr. 2.4851,

Inconel 625 / UNS N06625 / DIN W. Nr. 2.4856,Inconel 725 / UNS N07725,Inconel X-750 / UNS N07750 / DIN W. Nr. 2.4669,Inconel 600 / UNS N06600 / DIN W. Nr. 2.4816

Incoloy: Incoloy 800/800H/800HT/825/925/926;

GH: GH2132,GH3030,GH3039,GH3128,GH4180,GH3044

Monel: Monel 400/K500/R405

Nitronic: Nitronic 40/50/60;

Nimonic: Nimonic 75/80A/90/A263 ;

Specification Wire: 0.01-10mm

Strip: 0.05*5.0-5.0*250mm

Bar: φ4-50mm;Length 2000-5000mm

Pipe: φ6-273mm;δ1-30mm;Length 1000-8000mm

Sheet: δ 0.8-36mm;Width 650-2000mm;Length 800-4500mm

Product

Characteristics 1.According to the preparation process can be divided into deformation superalloys,

casting superalloys and powder metallurgy superalloys.

2.According to the strengthening mode, there are solid solution strengthening type, precipitation

strengthening type, oxide dispersion strengthening type and fiber strengthening type, etc..

Standard GB,AISI,ASTM,DIN,EN,SUS,UNS etc

Inspection ISO,SGS,BV and so on.

Application High temperature components such as turbine blades, guide vanes, turbine disks, high pressure

compressor disks,machine manufacturing

and combustion chambers used in the manufacture of aviation, naval and industrial gas turbines

Packaging 1. cases packed in wooden cases

2. paper packaging

3. plastic packing

4. foam packaging

Packaging according to customer requirements or products

Delivery 7-25days orAccording to the product

Payment L/C,D/A,D/P,T/T,Western Union,MoneyGram,According to customer requirements payments

for offline orders.

detail4


Varieties

Steel type

Specifications

(mm)

Precision
alloy
Resistance Alloys for electrical heating Super alloy Welding Wire Corrosion resistant
alloy
Rods hot rolling rods Φ8~38mm available available available
Cold-drawn rods ≤50mm available available available
Forged rods Φ38~350mm available available available
Wires Round wires Φ0.3~8mm available available available available available
Non-circle wires Negotiation available available available
Strips Cold rolling 0.15~4×200mm available available available available
Hot rolling 4~22×200mm available available available available
Plates Cold rolling 0.5~4×1000×2000mm available available available
Hot rolling 4~22×1000×2000mm available available available
tubes Φ4~63×0.5~5mm available available
Executive standard: GB, GJB, HB, YB, ASTM, AMSE, negotiation and so on.
Stainless Steel 3Stianless Steel 2Stainless Steel 1Stainless Steel 7Stainless Steel 6Stainless Steel 5AlloyStainless Steel 4

Looking for ideal Nimonic Alloy 80A Bar Manufacturer & supplier ? We have a wide selection at great prices to help you get creative. All the 80A Round Bar Rod are quality guaranteed. We are China Origin Factory of 80A Round Bar. If you have any question, please feel free to contact us.

Product Categories : Deforming Superalloy

Email to this supplier
  • *To:
    Mr. Allen Zhu
  • *Message:
    Your message must be between 20-8000 characters
Allen Zhu

Mr. Allen Zhu

SEND INQUIRY

  • Tel:

    +86-523-86550001

  • Fax:

    +86-523-81550001

  • E-mail:

    info@seonjip.com

Home

Product

Phone

About Us

Inquiry